Application Field
It is mainly used to determine the creep performance and endurance strength of metal materials under a certain temperature and constant load within a specified time.
Implement standard GB/T2039-1997 “Metal Tensile Creep and Endurance Test Method”, JJG276-88 “Verification Regulations for High Temperature Creep and Endurance Strength Testing Machine”.
Key Features
The standard description of the high temperature creep and endurance strength testing machine is used to determine the high temperature creep and endurance strength performance of metal materials under the conditions of constant temperature and constant tensile force in the axial direction of the sample.
Technical Features
Configure the corresponding accessories to achieve:
(1) High temperature endurance strength test:
A. Equipped with high temperature test device and temperature control system,
B. Equipped with permanent pull rod (specimen clamp),
C. The durable strength of the material can be measured under the action of constant temperature and constant tensile load.
(2) High temperature creep test:
A, equipped with high temperature test device and temperature control system,
B, equipped with high temperature creep pull rod (sample fixture)
C, equipped with creep extensometer (deformation drawing device)
D, equipped with creep measuring instrument (deformation measuring instrument).
The creep properties of materials can be measured under constant temperature and constant tensile load.
Model |
RDL-1250W |
Maximum load |
50KN |
Measuring force range |
1%-100% |
Test force accuracy grade |
0.50% |
Displacement accuracy |
±0.5% |
Speed range |
1*10-5—1*10-1mm/min |
Speed accuracy |
±0.5% |
Effective stretching distance |
200mm |
Manually adjustable moving distance |
50mm 4mm/revolution |
Effective test width |
400mm |
Sample |
round sample φ5×25mm, φ8×40mm |
Related Product Guide:
Innovation, excellent and reliability are the core values of our business. These principles today extra than ever form the basis of our success as an internationally active mid-size company for Excellent quality Multiaxial Creep Testing - RDL-1250W Computer controlled high temperature creep strength testing machine – Chengyu , The product will supply to all over the world, such as: Nigeria, Nigeria, Germany, As a way to use the resource on the expanding info in international trade, we welcome prospects from everywhere on the web and offline. In spite on the high quality objects we offer you, effective and satisfying consultation service is supplied by our qualified after-sale service group. Item lists and in depth parameters and any other info weil be sent to you timely for the inquiries. So you should make contact with us by sending us emails or call us when you've got any questions about our organization. ou could also get our address information from our site and come to our enterprise. We get a field survey of our merchandise. We're confident that we are going to share mutual accomplishment and create solid co-operation relations with our companions within this market place. We're seeking forward for your inquiries.