High definition Creep Testing Systems - RDL-1250W Computer controlled high temperature creep strength testing machine – Chengyu Detail:
Application Field
It is mainly used to determine the creep performance and endurance strength of metal materials under a certain temperature and constant load within a specified time.
Implement standard GB/T2039-1997 “Metal Tensile Creep and Endurance Test Method”, JJG276-88 “Verification Regulations for High Temperature Creep and Endurance Strength Testing Machine”.
Key Features
The standard description of the high temperature creep and endurance strength testing machine is used to determine the high temperature creep and endurance strength performance of metal materials under the conditions of constant temperature and constant tensile force in the axial direction of the sample.
Technical Features
Configure the corresponding accessories to achieve:
(1) High temperature endurance strength test:
A. Equipped with high temperature test device and temperature control system,
B. Equipped with permanent pull rod (specimen clamp),
C. The durable strength of the material can be measured under the action of constant temperature and constant tensile load.
(2) High temperature creep test:
A, equipped with high temperature test device and temperature control system,
B, equipped with high temperature creep pull rod (sample fixture)
C, equipped with creep extensometer (deformation drawing device)
D, equipped with creep measuring instrument (deformation measuring instrument).
The creep properties of materials can be measured under constant temperature and constant tensile load.
Model |
RDL-1250W |
Maximum load |
50KN |
Measuring force range |
1%-100% |
Test force accuracy grade |
0.50% |
Displacement accuracy |
±0.5% |
Speed range |
1*10-5—1*10-1mm/min |
Speed accuracy |
±0.5% |
Effective stretching distance |
200mm |
Manually adjustable moving distance |
50mm 4mm/revolution |
Effective test width |
400mm |
Sample |
round sample φ5×25mm, φ8×40mm |
Related Product Guide:
To be a result of ours specialty and repair consciousness, our corporation has won a good popularity amid consumers everywhere in the environment for High definition Creep Testing Systems - RDL-1250W Computer controlled high temperature creep strength testing machine – Chengyu , The product will supply to all over the world, such as: Colombia, Brasilia, Greek, We welcome you to visit our company, factory and our showroom displayed various products that will meet your expectation, meanwhile, it is convenient to visit our website, our sales staff will try their efforts to offer you the best service. If you need to have more information, remember to do not hesitate to contact us by E-mail or telephone.
By Quintina from Surabaya - 2017.02.28 14:19
The manufacturer gave us a big discount under the premise of ensuring the quality of products, thank you very much, we will select this company again.
By Barbara from Philadelphia - 2017.10.25 15:53