High definition Creep Testing Systems - RDL-1250W Computer controlled high temperature creep strength testing machine – Chengyu Detail:
Application Field
It is mainly used to determine the creep performance and endurance strength of metal materials under a certain temperature and constant load within a specified time.
Implement standard GB/T2039-1997 “Metal Tensile Creep and Endurance Test Method”, JJG276-88 “Verification Regulations for High Temperature Creep and Endurance Strength Testing Machine”.
Key Features
The standard description of the high temperature creep and endurance strength testing machine is used to determine the high temperature creep and endurance strength performance of metal materials under the conditions of constant temperature and constant tensile force in the axial direction of the sample.
Technical Features
Configure the corresponding accessories to achieve:
(1) High temperature endurance strength test:
A. Equipped with high temperature test device and temperature control system,
B. Equipped with permanent pull rod (specimen clamp),
C. The durable strength of the material can be measured under the action of constant temperature and constant tensile load.
(2) High temperature creep test:
A, equipped with high temperature test device and temperature control system,
B, equipped with high temperature creep pull rod (sample fixture)
C, equipped with creep extensometer (deformation drawing device)
D, equipped with creep measuring instrument (deformation measuring instrument).
The creep properties of materials can be measured under constant temperature and constant tensile load.
Model |
RDL-1250W |
Maximum load |
50KN |
Measuring force range |
1%-100% |
Test force accuracy grade |
0.50% |
Displacement accuracy |
±0.5% |
Speed range |
1*10-5—1*10-1mm/min |
Speed accuracy |
±0.5% |
Effective stretching distance |
200mm |
Manually adjustable moving distance |
50mm 4mm/revolution |
Effective test width |
400mm |
Sample |
round sample φ5×25mm, φ8×40mm |
Related Product Guide:
We generally continually give you quite possibly the most conscientious shopper company, and the widest variety of designs and styles with finest materials. These endeavours include the availability of customized designs with speed and dispatch for High definition Creep Testing Systems - RDL-1250W Computer controlled high temperature creep strength testing machine – Chengyu , The product will supply to all over the world, such as: Portugal, Grenada, Cancun, With the highest standards of product quality and service, our products have been exported to more than 25 countries like the USA, CANADA, GERMANY, FRANCE, UAE, Malaysia and so on.We are very pleased to serve customers from all over the world!

The customer service staff is very patient and has a positive and progressive attitude to our interest, so that we can have a comprehensive understanding of the product and finally we reached an agreement, thanks!