Wholesale High Temperature Creep Testing Machine - RDL-1250W Computer controlled high temperature creep strength testing machine – Chengyu


Specification

Related Video

Feedback (2)

We have been also specializing in improving the things administration and QC system to ensure that we could preserve terrific gain within the fiercely-competitive company for Plastic Impact Tester, Spring Testing Instrument, Pendulum Impact Testing Equipment, For high quality gas welding & cutting equipment supplied on time and at the right price, you can count on company name.
Wholesale High Temperature Creep Testing Machine - RDL-1250W Computer controlled high temperature creep strength testing machine – Chengyu Detail:

Application Field

It is mainly used to determine the creep performance and endurance strength of metal materials under a certain temperature and constant load within a specified time.

Implement standard GB/T2039-1997 “Metal Tensile Creep and Endurance Test Method”, JJG276-88 “Verification Regulations for High Temperature Creep and Endurance Strength Testing Machine”.

Key Features

The standard description of the high temperature creep and endurance strength testing machine is used to determine the high temperature creep and endurance strength performance of metal materials under the conditions of constant temperature and constant tensile force in the axial direction of the sample.

Technical Features

Configure the corresponding accessories to achieve:

(1) High temperature endurance strength test:

A. Equipped with high temperature test device and temperature control system,

B. Equipped with permanent pull rod (specimen clamp),

C. The durable strength of the material can be measured under the action of constant temperature and constant tensile load.

(2) High temperature creep test:

A, equipped with high temperature test device and temperature control system,

B, equipped with high temperature creep pull rod (sample fixture)

C, equipped with creep extensometer (deformation drawing device)

D, equipped with creep measuring instrument (deformation measuring instrument).

The creep properties of materials can be measured under constant temperature and constant tensile load.

img (2)

Model

RDL-1250W

Maximum load

50KN

Measuring force range

1%-100%

Test force accuracy grade

0.50%

Displacement accuracy

±0.5%

Speed range

 1*10-5—1*10-1mm/min

Speed accuracy

±0.5%

Effective stretching distance

 200mm

Manually adjustable moving distance

50mm 4mm/revolution

Effective test width

400mm

Sample

round sample φ5×25mm, φ8×40mm


Related Product Guide:

We retain bettering and perfecting our merchandise and service. At the same time, we do the job actively to do research and improvement for Wholesale High Temperature Creep Testing Machine - RDL-1250W Computer controlled high temperature creep strength testing machine – Chengyu , The product will supply to all over the world, such as: Singapore, Jordan, Algeria, Based on products with high quality, competitive price, and our full range service, we have accumulated professional strength and experience, and we have built up a very good reputation in the field. Along with the continuous development, we commit ourselves not only to the Chinese domestic business but also the international market. May you moved by our high quality products and passionate service. Let's open a new chapter of mutual benefit and double win.
This supplier offers high quality but low price products, it is really a nice manufacturer and business partner.
5 Stars By Andy from Venezuela - 2018.02.12 14:52
The company can think what our think, the urgency of urgency to act in the interests of our position, can be said this is a responsible company, we had a happy cooperation!
5 Stars By Sandra from Florence - 2018.08.12 12:27
Write your message here and send it to us